    Keamppi 1500 mastertig -problem
    hi all
    i need one informations about my ,,Kemppi 1500mastertig .
    what it is values to all resistor RZ101,102,103 -PCB Z001?
    SEE in the pictures .
    the first pictures
    [​IMG]

    Uploaded with ImageShack.us
    second pictures .
    [​IMG]

    Uploaded with ImageShack.us

    Best regardes
    WAIT YOUR ANSWER
    IOAN
    KN35 AJ
     
  2. Gargouille07

    Gargouille07 Nouveau

    Messages:
    12
    Inscrit:
    6 Mai 2009
  3. IOAN

    IOAN Nouveau

    Messages:
    8
    Inscrit:
    5 Février 2013
    Localité:
    ROMANIA -KN35 AJ
    Keamppi 1500 mastertig -problem
    ok dear men ,
    I fix all problem the principal defeckt it was ,, filter T,, so 220v/50hz burn all varistors (varistor it is important protection for high voltaje).
    But I mistake when positions gate igtb and result burn igtb ,I change igtb and position correct all gates igtb.
    In this moment my ,,KEMPPI MASTERTIG 1500,, good function but not start coller.
    I chek with 12v/dc coller it is good function .
    I supouse not arivve signal for start coller .
    Please tell me you have one idea whay not function my cooler ?
    BEST REGARDES
    IOAN -I wait you replay
     
  4. Gargouille07

    Gargouille07 Nouveau

    Messages:
    12
    Inscrit:
    6 Mai 2009
    Keamppi 1500 mastertig -problem
    Hello.

    What do you mean by : good function but not start coller?
    Have you checked rectifier diodes?
    Bye.
     
  5. IOAN

    IOAN Nouveau

    Messages:
    8
    Inscrit:
    5 Février 2013
    Localité:
    ROMANIA -KN35 AJ
    Keamppi 1500 mastertig -problem
    hi and sory not speak very good English
    So ,my coller not start
    I weld probe maximal 1 minuntes ,but not start coller .
    I waiting your replay.
    BEST REGARDES
    IOAN
     
  6. Gargouille07

    Gargouille07 Nouveau

    Messages:
    12
    Inscrit:
    6 Mai 2009
  7. IOAN

    IOAN Nouveau

    Messages:
    8
    Inscrit:
    5 Février 2013
    Localité:
    ROMANIA -KN35 AJ
    Keamppi 1500 mastertig -problem
    hi ,
    Is it right I welder only 1 minunte, because, I consider very dangers for my ,,kemppi,,
    I wait your replay.
    IOAN
     